Our Products

Bismuth Telluride Doped – Based Composite Thermoelectric Materials (Purity: 99.99%, APS: 20-30µm)

Categories: ,

Bismuth Telluride Doped – Based Composite Thermoelectric Materials (Purity: 99.99%, APS: 20-30µm)

Bismuth Telluride Doped – Based Composite Thermoelectric Materials (Purity: 99.99%, APS: 20-30µm)
Product No. CAS Purity APS Type Melting Point Appearance Thermal Conductivity
NRE-31010 1304-82-1 99.99% <30µm (can be customized) N-type 586 °C Grey powder 1.2-1.6w/m.K
Molecular Weight 800.76 g/mol
Molecular Formula BiTe3-0.1
Density 7.642 g/cm³