Our Products

Lead Telluride Selenium Doped Thermoelectric Materials (Purity :99.99%, APS: 20-30µm)

Categories: ,

Lead Telluride Selenium Doped Thermoelectric Materials (Purity: 99.99%, APS: 20-30µm)

Lead Telluride Selenium Doped Thermoelectric Materials (Purity: 99.99%, APS: 20-30µm)
Product No. CAS Purity APS Formula Molecular Weight Density Color
NRE-31061 1314-91-6 99.99% <30 µm (can be customized) PbTe (0.9+0.1) Se0.1 334.80 g/mol 18.164 g/cm³ Gray powder
Doping Selenium (Se) Doped
Melting Point 924 °C
Boiling Point NA
Certificate of Analysis

Cu

Fe

Pb

Ag

Cd

As

Ti

Zn

Sn

Mn

Al

Bi

3ppm

14ppm

5ppm

5ppm

6ppm

11ppm

2ppm

1ppm

5ppm

5ppm

2ppm

1ppm

Lead Telluride Selenium Doped Thermoelectric Materials